就爱看肏屄免费视频在线|亚洲熟人妇一区二区三区|国产黄色电影免费在线观看|一区二区三区免费电影|精品一级A片一区二区免费视频看|国产αV精品观看|91拍真实国产伦偷精品|欧美韩国三级日本费一页高清|国产无码精品AV在线|97成人网sss

qxdali
錫礦選礦工藝

Tin

Tin processing usually adopts gravity separation. However, iron oxides such as magnetite and hematite are often associated with tins, so it is impossible to completely separate the ore by gravity separation alone. Magnetic separation and flotation are also used in tin ore processing. Chat With Us Leave Message

Various tin minerals, such as sulphur-tin-lead ore, stibnite-tin-lead ore, cylindrical tin ore, black sulphur-silver-tin ore, black boron-tin ore, cassiterite, magnesite-tin ore, etc.

錫礦選礦工藝1

  1. Washing and Desliming

This step is aimed at the raw ore with large mud content and strong cementation, which should be washed and desliming before crushing

  1. Crushing and Screening

Crush the ores to be size less than 20mm. Then divide into 0-4mm and 4-20mm by vibration screen.

  1. Pre-separation

The 4-20mm size ores are pre-separated by hydrocyclone, and then they enter grinding mill. After being grinded, the ores are further separated by jigger and vibrating screen. The screening size is controlled at 2mm. The ores of size less than 2mm separated by shaking table, and the ores of size above 2mm become tailings.

  1. Flotation

The flotation stage is divided into two steps: mixed flotation and separation flotation. Firstly, the concentrate separated by jigger and shaking table should be processed through mixed flotation. Then the concentrate of mixed flotation should be flotation-processed to remove lead-zinc, and the tin in the tailings should be separated by shaking table to produce qualified tin concentrate.

  1. Gravity Separation

Slime enters the 300mm hydrocyclone, and the fine sludge is removed by 125mm and 75mm hydrocyclones after overflow. Cassiterite flotation is carried out after concentration and flotation desulfurization of sediment.